Hydrogen cracking in metastable austenitic stainless steels
An illustration of cracking associated with the hydrogen embrittlement of austenitic stainless steel that is pulled in tension. It is clear that in both cases, cracking occurs at many locations other than at the artificial notch (stress concentration) at the centre. This is because of thermal-induced, deformation-induced martensite and deformation bands.
Koyama M, Ogawa T, Yan D, Matsumoto Y, Tasan CC, Takai K, Tsuzaki K. Hydrogen desorption and cracking associated with martensitic transformation in Fe-Cr
2 views
7392
3385
6 years ago 00:01:13 2
Hydrogen cracking in metastable austenitic stainless steels
5 years ago 00:00:46 36
Space Launch System Liquid Hydrogen Tank Test
2 years ago 00:20:15 1
Solid Hydrogen Explained (Again) - Is it the Future of Energy Storage?
1 year ago 00:13:20 1
Mercedes-Benz GenH2 Truck Hydrogen Record Run (1000 km) {Germany, September 2023}
4 years ago 00:51:58 4
Master Cracker Ear Cleaning Head Massage and Neck Cracking | Indian Massage
2 years ago 00:30:03 1
DIY Hydrogen/Oxygen Generators From Grocery Store Items (HHO Fuel Cells & Split Cell Electrolysis)
2 years ago 00:30:02 3
Lee Hangjun, Hong Chulki - Cracked share - 2006
2 years ago 00:04:51 1
It took 80 Years And The World’s Greatest Chemists
11 years ago 00:03:21 10
Exploding Egg - Cool Science Demo
2 years ago 00:23:06 4
How This Fusion Reactor Will Make Electricity by 2024
3 years ago 00:12:26 1
Growing Passion Fruit from Seeds, Days 0-100
2 years ago 00:02:19 9
4K The Arkansas Battleship Was Lifted Upwards By Underwater Nuclear Blast Closest Footage 1946
1 year ago 00:03:37 1
SMOKEY JOE & THE KID - Beast On Beat (Feat. R.A The Rugged Man) - Official Visualizer
1 year ago 00:30:58 1
NASA SPACE SHUTTLE RS-25 SPACE SHUTTLE MAIN ENGINE SSME TESTS & FAILURES FILM XD13604
8 months ago 00:10:40 1
Xiaomi builds the SU7 in 76 seconds using worlds biggest gigacasting machine
10 months ago 00:06:31 1
A cheap electrolyte gel gives lithium batteries 40% more energy density